Differential Scanning Calorimeter (DSC) Q100

Instrument types
Make / Model : 

(DSC) Q100

The DSC measures temperatures and heat flows associated with thermal transitions in a material. Properties measured by DSC techniques include heat capacity at different temperatures, parameters of glass transitions, phase changes (melting, crystallization), product stability, cure/cure kinetics.